#1
|
|||||
|
|||||
![]() Weld On #16 has good gap filling qualities so if your cuts are a bit loose it will work fine. For a good solid joint use #3 (dries very fast) or #4 (bit more open time). Your joints have to be tight with these two as they have the consistency of water.
Weld On is the only stuff I use and I've built a good number of sumps.
__________________
250 gal display tank plumbed directly to my wallet |
#2
|
|||||
|
|||||
![]() Yuppers Weld on #16,3,4 is the only stuff that i have used, and you can get it from any Glass company, where they build acrylic stuff along with glass,...
__________________
180 starfire front, LPS, millipora Doesn't matter how much you have been reading until you take the plunge. You don't know as much as you think. |
#3
|
|||||
|
|||||
![]() thanks everyone
Super7 |