![]() I was cleaning my glass today and noticed a tiny bubble on the front glass. Smaller than an oxygen bubble. So I tried to wipe it off when I noticed it is inside the glass. Could this be a weak point that could lead to the pane cracking?
I have only had the tank running 3 weeks and bought it used without any scratch at all. It could be that this was always there or that it just happened. My main concern is could it lead to a crack? Both sides inside and outside are smooth so this is in the glass. |
#2
|
||||
|
||||
![]() some sort of hiccup in the manufacturing process would be my guess. i cant see it being much of an issue unless it was experiencing rapid and extreme temperature changes...
__________________
![]() - 33 Gal - 20Gal Sump, MP10/Hydor Powerheads, Aquaticlife 4x T-5HO, Vertex IN100, TLF w/Biopellets, Tunze ATO -45GAL Build in Progress!- |
#3
|
||||
|
||||
![]() Great thanks.
|
#4
|
|||||
|
|||||
![]() Sometimes referred to as a 'seed'. Its definitely a defect in the glass manufacturing. Unless it is huge... it shouldnt be an issue!
__________________
No more tanks ![]() Cheers, Chris |
#5
|
||||
|
||||
![]() About the size of a tiny air bubble. Smaller than the head of a pin.
|
#6
|
|||||
|
|||||
![]() I wouldn't worry about it.
__________________
![]() Setup: 180G DT, 105G Refuge (approx. 300lbs LR, 150lbs Aragonite) Hardware: Super Reef Octopus SSS-3000, Tunze ATO, Mag 18 return, 2x MP40W, 2X Koralia 4's Wavemaker Lighting: 5ft Hamilton Belize Sun (2x250W MH, 2X80W T5HO) Type of Aquarium: mixed reef (SPS & LPS) with fish Dosing: Mg, Ca, Alk |
![]() |