![]() i have been looking into building a skimmer lately and have priced out some 6" acrylic tubing all 1/8" and if you buy a 6' length from industrial paints and plasitcs in Calgary they will sell it to you for 105$ nearly halfs your main chamber costs.
they are located in the industrial park in the s.e. near chinook center, they also had the 6" in stock when i was there last wednesday. also i found a site on the internet www.k-mac-plastics.com they aslo sell the acrylic tube for less then you say you can get it IF you buy in a 6' lengths. hope this helps you some. Richard |
#2
|
|||||
|
|||||
![]() Kari, you can guinea pig us any time. We will pay for anything that makes life/tanks better...
![]() ![]()
__________________
http://www.canreef.com/ftotm/sept05/index.php |
#3
|
|||||
|
|||||
![]() That horizontal design is very interesting, I say definately build a test unit. It just might be the ticket.
|
#4
|
||||
|
||||
![]() Quote:
Thanks for the input though. |
#5
|
|||||
|
|||||
![]() Kari, have you actually had extruded crack on you? I ask because I've always built my skimmers and reactors from extruded, anywhere from 4" to 8" tubing, and as far as I know, pieces built 7 years ago are still in service. My Ca Reactor has been around for 5 years and the LFS is using one of my first skimmers built 7 years ago. I know it's not as clear, but it's always stayed crack free and not leaked. Just wondering if your experiences have been different?
__________________
Brad |
#6
|
|||||
|
|||||
![]() brad what thickness extrudes did you use? I've used up to 1/8 extruded and it cracks like crazy (fine cracks where glue was applied)
__________________
____________ If people don't die, it wouldn't make living important. And why do we fall? So we can learn to pick ourselves up. |
#7
|
|||||
|
|||||
![]() I've used both 1/8 and 1/4, never had anything crack. You might see some crazing around seams, but no cracks. Maybe the material these days is crappier than 5 years ago? Dunno, just always used extruded
__________________
Brad |
#8
|
||||
|
||||
![]() Quote:
|
#9
|
|||||
|
|||||
![]() Quote:
I never got much crazing, but all my joints were just plain old straight edges. I wonder if different suppliers have different grades? I got my tubing at a local shop, not IPP
__________________
Brad |
#10
|
||||
|
||||
![]() There is a lot of really informative but dry reading in the tech support area at one of the acrylic manufacturers site (Cyro) for info on this subject. One would need to create a user name to get at it.
http://cyro.custhelp.com/cgi-bin/cyr...ge=std_alp.php . |
![]() |