Ok, so today's lesson is: flame-polishing is NOT the method of choice for getting an optically clear finish on a 0.075" thick microtank. What a pain in the freakin' ass that was. Never the less, I was successful (or about as successful as I cared to be).

So here's the tank after it's first test fill (you know, I don't want any major water disasters all over the floor when this bad boy gets up and running) with it's big brother in the background for perspective.

(I should have wiped the finger prints off for this pics...)


And here's another pic... for fun!